Is there a correlation between relative humidity percentage and moisture vapor emission rate measured with calcium chloride testing?

Follow

There is no correlation between the tests. Relative humidity testing is a measure of moisture condition in the concrete. When a floor covering is placed on top of a slab, it restricts evaporation from the top surface of the slab; moisture within the slab then distributes itself to achieve equilibrium due to temperature and chemical interactions from the top to the bottom of the slab. In the long run, adhesive and flooring are then exposed to the equilibrium moisture condition at the top of the slab. The calcium chloride test does not reflect the long-term moisture situation that will be established by equilibration and can even artificially pull moisture out of the top few centimeters of the slab. Rapid RH® 4.0 EX Smart Sensors measure the relative humidity that will exist after the floor is covered. See chart on measuring at the correct depth

Please call 1.800.634.9961 to talk to a professional if you should need more information.

Have more questions? Submit a request

Comments

Powered by Zendesk