How many relative humidity tests should I use on each job?

Follow

For the Flooring Contractor and as part of the project documentation process, ASTM F2170 requires that 3 tests be placed in the first 1,000 sq. ft. and one test be placed every 1,000 sq. ft. thereafter. If you are using the Rapid RH® system as a monitoring tool early in a project to determine when final acceptance testing should be performed, several Rapid RH® 4.0 EX Smart Sensors can be placed throughout the floor 28 days after the pour and readings taken as often as desired. 

Please visit http://bit.ly/1d5SFVL for more information or call 1.800.634.9961 to talk to a professional.

 