How many probes do I use?

Follow

In accordance with ASTM F2170-11, you should use:

  • 3 Smart Sensors (aka probes, sensor barrels) must be used for first 1,000 square feet.
  • 1 Smart Sensor for every additional 1,000 square feet.
  • If your slab is 1,200 square feet then you would need 4 probes.

 

 Square Feet

Number of
Smart Sensors

0 - 1,000       3  
1,001 - 2,000     4
2,001 - 3,000     5
3,001 - 4,000     6
4,001 - 5,000     7
5,001 - 6,000     8
6,001 - 7,000     9
7,001 - 8,000     10
8,001 - 9,000     11
9,001 - 10,000  

  12

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 