40% Drill Depth Measurements Chart

Follow
Slab
Thickness
Drill Depth
1/10ths
Drill Depth
1/16ths
3" 1.2" 1 3/16"
4" 1.6" 1 5/8"
5" 2" 2"
6" 2.4" 2 3/8"
7" 2.8" 2 13/16"
8" 3.2" 3 3/16"
9" 3.6" 3 10/16"
10" 4" 4"
11" 4.4" 4 3/8"
12" 4.8" 4 13/16"

 

Please visit http://bit.ly/1iVnZJi and http://bit.ly/1dsvYfv for more information or call 1.800.634.9961 to talk to a professional.